Fuel Gas
Tables for LP [Liquefied Petroleum] Gas System
Capacities in these tables are based on the properties of commercial propane gas (LP) with a specific gravity of 1.52. Physical properties of the gas are based on those properties given in the Gas Processors Suppliers Association Engineering Data Book, Eleventh Edition.
Table 3LP - Maximum Capacity* for the Flow of Undiluted LP Gases Through Copper Tube in a Low Pressure System of Less than 14 inches wc and Pressure Drop of 0.5 inches wc, CFH.**
Table 4LP - Maximum Capacity* for the Flow of Undiluted LP Gases Through Copper Tube in a Low Pressure System of Less than 14 inches wc and Pressure Drop of 1 inch wc, CFH.**
Table 5LP - Maximum Capacity* for the Flow of Undiluted LP Gases Through Copper Tube in an Elevated Pressure System of 2 psig and Pressure Drop of 1.0 psig., CFH.** (Based on atmospheric pressure at sea level.)
Table 6LP - Maximum Capacity* for the Flow of Undiluted LP Gases Through Copper Tube in an Elevated Pressure System of 5 psig and Pressure Drop of 3.5 psig, CFH.** (Based on atmospheric pressure at sea level.)
Table 8LP - Maximum Capacity* for the Flow of Undiluted LP Gases Through Copper Tube in a Low Pressure System of Less than 14 inches wc and Pressure Drop of 2.5 inches wc, CFH.**
Notes:
* Includes a 20% factor for fittings
** See Table 7.
Useful Resources
Table 1 Copper Tube: For Gas Installation
Type K |
Type L
ACR | Type Gas
Table 2 Dimensions and Physical Characteristics of Copper Tube: TYPES K, L, ACR and Gas.
Table 3 Maximum Capacity for Copper Tube in a Low Pressure System of Less than 14 inches wc and Pressure Drop of 0.5 inches wc, CFH.
Table 4 Maximum Capacity for Copper Tube in a Low Pressure System of Less than 14 inches wc and Pressure Drop of 1 inch wc, CFH.
Table 5 Maximum Capacity for Copper Tube in an Elevated Pressure System of 2 psig and Pressure Drop of 1.0 psig., CFH. (Based on atmospheric pressure at sea level.)
Table 6 Maximum Capacity for Copper Tube in an Elevated Pressure System of 5 psig and Pressure Drop of 3.5 psig, CFH. (Based on atmospheric pressure at sea level.)
Table 7 Multipliers to be Used with Tables 3 through 6 When Specific Gravity of Gas is Other than 0.60.
Table 3LP Maximum Capacity for the Flow of Undiluted LP Gases Through Copper Tube in a Low Pressure System of Less than 14 inches wc and Pressure Drop of 0.5 inches wc, CFH.
Table 4LP Maximum Capacity for the Flow of Undiluted LP Gases Through Copper Tube in a Low Pressure System of Less than 14 inches wc and Pressure Drop of 1 inch wc, CFH.
Table 5LP Maximum Capacity for the Flow of Undiluted LP Gases Through Copper Tube in an Elevated Pressure System of 2 psig and Pressure Drop of 1.0 psig., CFH. (Based on atmospheric pressure at sea level.)
Table 6LP Maximum Capacity for the Flow of Undiluted LP Gases Through Copper Tube in an Elevated Pressure System of 5 psig and Pressure Drop of 3.5 psig, CFH. (Based on atmospheric pressure at sea level.)
Table 8LP Maximum Capacity for the Flow of Undiluted LP Gases Through Copper Tube in a Low Pressure System of Less than 14 inches wc and Pressure Drop of 2.5 inches wc, CFH.